Compare |
Performance |
Powder expory |
Liquid epoxy |
Raw material |
Solvent-free, food grade powder, green |
Diluent, curing agent, irritating odor |
Process |
Hot melting spraying, make an action with the steel pipes in 250 degree forming a alloy layer with steel and plastic |
Cold spray by spray gun, need time for curing |
Adhesive force |
Mechanical chimeric, chemical bonds, diffusion, electrostatic binding force |
Mechanical chimeric |
Thickness / each time |
300-500μm |
30-80μm |
Friction coefficient |
0.0086 |
0.012 |
Time for using in theory |
50 years |
3 - 5 years |